dc.description.abstractCompression testing of Ti-6Al-4V alloy has been carried out at temperatures between 303 K to 873 K. To prevent embrittlement due to atmospheric oxygen and nitrogen, the samples were given a glass coating, which also acts as a lubricant simultaneously. Dynamic Strain Aging was observed to occur in the temperature range of 600 K to 800 K. Below 600 K stresses were high. Warm working has to be done above 800 K but below 1163 K (0.6 Tm where Tm = 1940 K) which is the recrystallization temperature. Based on these conclusions, warm extrusion has been successfully carried out in the Materials Forming Laboratory of I.I.T., Madras, Chennai, India.en_US
dc.titleCompression testing of Ti-6Al-4V in the temperature range of 303-873 Ken_US
dc.typeArticleen_US
Appears in Collections:1. Journal Articles

Files in This Item:
File Description SizeFormat 
10317.pdf936 kBAdobe PDFThumbnail
View/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.